Measure each battery with a voltmeter after the cart has sat unplugged for a few hours, then type the readings in below. The checker shows how charged each battery is and which one is weak, using the voltage tables and the 0.3 volt rule the battery makers publish.

Batteries give off explosive hydrogen gas. Keep sparks and flames away, wear safety glasses, and never lay a tool across two terminals.

Your battery pack

Count the batteries under the seat and read the voltage printed on one of them. Not sure? See 6 V, 8 V and 12 V packs.

Trojan asks for at least 6 hours of rest, 24 if you can wait; U.S. Battery asks for 24 hours on AGM batteries. A fresh reading straight off the charger looks better than the battery is.

Voltage of each battery

Set the meter to DC volts and put the probes on one battery's positive and negative posts. Number the batteries in the order you measure them (a strip of tape helps).

Optional: hydrometer readings for one battery

Flooded batteries only. Draw a sample from each cell of the battery you suspect and enter the readings with the electrolyte temperature.

How the checker reads your numbers

Each reading is matched against U.S. Battery's state of charge table for flooded and AGM batteries, with the charge worked out between the published 10 percent steps. Trojan's battery maintenance table prints the same full-charge voltages for flooded batteries.

Charge6 V flooded8 V flooded12 V flooded12 V AGM
100%6.37 V8.49 V12.73 V13.00 V
70%6.19 V8.25 V12.37 V12.62 V
50%6.05 V8.07 V12.10 V12.37 V
0%5.68 V7.57 V11.35 V11.74 V

The weak battery is found the way the makers describe it. Trojan's user guide says that if any battery reads more than 0.3 V apart from another in the set, equalize the set (flooded batteries only) and measure again, and that a gap still above 0.3 V may mean a failed battery. U.S. Battery and Crown print the same 0.3 V line. Trojan also says to charge any battery that reads 0 to 70 percent before judging it.

The hydrometer check corrects each reading to 80°F (add 0.004 for every 10°F above, subtract 0.004 for every 10°F below, as both makers print it). U.S. Battery calls a single cell more than 0.050 off the others a bad cell; Trojan says to equalize when the cells of one battery differ by more than 0.030, and U.S. Battery uses 0.015. Voltage is the least reliable of the tests by U.S. Battery's own account, so a battery the checker flags is worth confirming with a hydrometer or a load test before you replace it. The full method is on how to test golf cart batteries.